Guenter: "Sumitomo Product Data" 1999 => Plastic overmold CTE = 13.0 ppm/°C
Dave Fish
Guenter Grossmann wrote:
> Hi folks
>
> Can somebody provide the CTE of glob-top resins and of plastic IC packaging resins?
>
> Thanks a lot
>
> Guenter
>
> Guenter Grossmann
> Swiss Federal Institute for Materials Testing and Research EMPA
> Centre for Reliability
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax : xx41 1823 4054
> mail: [log in to unmask]
>
> ---------------------------------------------------------------------------------
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------