What is the SnAgCu eutectic? I have heard 3 or 4 different parties claim a
particular alloy to be the eutectic formulation while contradicting the work
of others. For my money, it seems like we'll never know with 100%
confidence, simply b/c a few parties are interested in touting their own
alloys. Furthermore, what does it really matter, as most SnAgCu alloys seem
to have only a 1-2C pasty range? After all, the tin/lead alloy we all refer
to as eutectic (Sn63/Pb37) is not the true eutectic, as any phase diagram
will prove.
David
----- Original Message -----
From: "<Erik de Kluizenaar>" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, October 24, 2000 1:39 PM
Subject: Re: [LF] Timelines for conversion to Lead-Free
Dear Mr. Han Jiangbo, dear all,
Europe as such does not make such a choice. There is no official body here
that would prescribe this. However, it is becoming common opinion throughout
the world, including Europe, that the SnAgCu eutectic alloy is the general
purpose lead-free solution.
WEEE has been adopted by the European Commission only. That is not the same
as adopted as a European law. It still is a draft. It has to go to the EU
parliament, and to the Board of Ministers of the member countries for
amendments and voting. This is a
trajectory that can easily take two years, and the contents can still be
changed.
Best regards, Erik
----------------------------------------------------------------------------
------------------------------------------------------
Erik E. de Kluizenaar
Philips CFT - Electronic Packaging & Joining (EP&J)
Building SAQ-p, p/o box 218, 5600 MD Eindhoven - The Netherlands
Tel/Fax: (+31 40 27) 36679/36815; E:mail [log in to unmask]
PHILIPS worldwide homepage: http://www.philips.com
Internal PHILIPS only:
http://pww.cft.philips.com/cfteurope/electronics/elpajo/index.htm
----------------------------------------------------------------------------
-------------------------------------------------------
[log in to unmask]@[log in to unmask] on 2000/10/24 06:00:06 AM
Please respond to [log in to unmask]@SMTP
Sent by: [log in to unmask]
To: [log in to unmask]@SMTP
cc:
Subject: Re: [LF] Timelines for conversion to Lead-Free
Classification:
Hi,
I would like to confirm two pieces of information.
(1) Europe has recommended NEMI's selection (SnAgCu) as the 'standard'
eutectic tin-lead solder replacement.
(2) EC WEEE proposal has been officially adopted.
Appreciate if anyone can help to clarify whether the above is true.
Best regards,
Han Jiangbo, Agilent Technologies
----------------------------------------------------------------------------
-----
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|