In a message dated 10/30/2000 4:13:48 PM US Eastern Standard Time,
[log in to unmask] writes:
> I am looking for some information on dry film soldermask vs. LPI
> soldermask.
From the studies we have done on cleanliness related issues, the only benefit
I see dryfilms having is the ability to tent. From a residue retention
aspect, LPIs win hands down.