Hi Michael
Before I would recommend looking for contamination, I would do some
solderability
testing of the components. Component lead solderability testing is pretty
straight forward and can imploy accelerated aging through steam prior to
testing. Then if
there was a problem, and depending on what the de-wet or non-wet areas looked
like would I continue with contamination testing.
Susan Mansilla
Robisan Lab
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------