Hiya folks, I have been approached by a company that are suggesting that we
use "Silver Through Hole" technology
instead of our usual PTH.
As a manufacturer of fire detection equipment I am concerned about
reliability and long life etc.
I am seeking others knowledge & experiences with this plating method.
Additionally we only ever use FR4, and it is being suggested to use FR4 &
CEM laminates and I would like
to know the good & bad features of these.
Many thanks :-
Matthew Lamkin
Printed Circuitboard Draughtsman
Protec Fire Detection PLC.
Protec Hse, Churchill way,
Nelson, Lancashire.
England UK. BB9 6RT
Email [log in to unmask]
(please only use this email address when sending to or replying to this
message)
Tel: 01282 717393 - Fax 01282 717273
Owner http://www.egroups.com/group/cadstarusers
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|