TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 1 Nov 2000 09:19:15 +0800
Reply-To:
刘常康 <[log in to unmask]>
Subject:
From:
刘常康 <[log in to unmask]>
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="UTF-8"
Organization:
Huawei Technology Co.,Ltd.
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Dear Engelmaier,

 Thank for your help.

 I think perfect fillet shows good wetting, and our product is communication equipment, and I am not sure that which is inportant between wetting and fill ratio.

 Can you give any more advice?

 

Best regards

Liu Changkang



----- Original Message ----- 

From: "Werner Engelmaier" <[log in to unmask]>

To: <[log in to unmask]>

Sent: Wednesday, November 01, 2000 12:55 AM

Subject: Re: [TN] Through-hole Solder Joint inspection and quality criteria





> In a message dated 10/31/0 4:12:07, [log in to unmask] writes:

> > One partly poor wetting component  after wave soldering, through-hole

> >solder joint shows good wetting near top side PCB, but show bad wetting

> >on the bottom side and through-hole is about 70% filled. some suggest good

> >wetting is key to evaluate a SJ reliability. IPC suggest 75% filled is

> >OK, which one I choose?

> >Same situation happen to  paste in hole process, Which type SJ is ok?

> >the key is the fill ratio or the good wetting?

> >If half of through hole SJ is good wetting, half of which is bad, Is it ok?

> 

> Hi Liu,

> Good wetting is by far the more important physical aspect--however, an

> incomplete fill may be a sign of wetting problems. Further, if you have

> "partly poor wetting", how do you know the rest is "good wetting"?

> If you have good wetting, a partial hole fill is only important in a severe

> use environment, e.g. automotive, because of the stress concentration on the

> PTH barrel at the solder/no-solder interface.

> 

> Werner Engelmaier

> Engelmaier Associates, L.C.

> Electronic Packaging, Interconnection and Reliability Consulting

> 7 Jasmine Run

> Ormond Beach, FL  32174  USA

> Phone: 904-437-8747, Fax: 904-437-8737

> E-mail: [log in to unmask], Website: www.engelmaier.com

> 

> ---------------------------------------------------------------------------------

> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d

> To unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet

> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives

> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional

> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315

> ---------------------------------------------------------------------------------


ATOM RSS1 RSS2