Thanks Doug
Douglas Pauls wrote:
> In a message dated 10/30/2000 3:58:02 PM US Eastern Standard Time,
> [log in to unmask] writes:
>
> > Continuing with your thoughts, we have been able to create white res on WS
> > fluxed boards by washing them blistering hot, straight out of the wave.
> So, even
> > when we were shrewd enough to control our was temps, we were still able to
> beat ourselves.
> > Tricky eh? Dave Fish
>
> You might be seeing the residual weak organic acids from the WS flux reacting
> with the water to turn white. In addition to what Brian Ellis has written,
> when we see white residues, it is either abietic acid from rosin turning
> white or weak organic acids from the flux turning white. The latter occurs
> more frequently with the low solids fluxes since they have a much higher
> level of WOAs.
>
> Doug Pauls
> CSL
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|