Dow Corning offers a "silicone Cleaner and Surface Prep Solvent" called
OS-2. Haven't tried it, though. If you do, please let me know how it
works.
Thanks,
Jim M.
-----Original Message-----
From: Ernie Crump [SMTP:[log in to unmask]]
Sent: Tuesday, October 31, 2000 2:59 PM
To: [log in to unmask]
Subject: [TN] Silicone
We have had a vendor use a silicone rubber mat on his platen while
bonding a
heatsink to a polymide pwb, and we suspect that the silicone has
become part of
the pwb surface on the one side, as the UR coating process has
produced
fisheyes, and peelable coating, just on the one side.
We use Bioact-7R, alcohol and then di water to clean in a proper
monitored pwb
washer, but the removal of silicone is very difficult.
What cleaners are recommended for removing it, without destroying
components, or
leaching under the bonded heatsink?
Thank you. Ernie Crump Raytheon Systems Canada.
Phone 519-885-0110, fax. 519-885-1178
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|