Franklin,
I think you may have misread Ken's message... It says "associated pads" not
"associated vias". An associated pad is the outer layer pad that is at each
end of the via hole.
Just my 2 cents,
Alain Savard, B.Sc.
Chemical Process Analyst
CAE Electronics Ltd.
e-mail: [log in to unmask]
-----Original Message-----
From: Franklin D Asbell [mailto:[log in to unmask]]
Sent: October 30, 2000 6:36 PM
To: [log in to unmask]
Subject: Re: [TN] Plugging (not tenting) of via fab notes
It's a little confusing...but then I'm not the expert.
In regards to exposed vias...the artwork will dictate what vias are to
be exposed and/or plugged so the mention of that in the notes may
confuse the issue. Stating Green LPI IAW SM-840 should be enough in most
cases I would suspect. Your comment on 'associated vias'...what exactly
are 'associated vias? Is this all vias on a commen net?
Hope the critique helps some.
Franklin
Ken Patel wrote:
>
> Fab Expert,
> Is the following fab note make sense to you or should I also
mention
> the plugging side as I do not want higher surface on fine-pitch side.
Also,
> comment on use of SR1000 epoxy in my fab note.
>
> SOLDERMASK: GREEN PHOTOIMAGEABLE, BOTH SIDES PER IPC-SM-840, CLASS
> 3. ALL TEST-VIAS AND ASSOCIATED PADS ARE TO BE FREE OF SOLDERMASK. ALL
> NON-TEST VIA HOLES TO BE PLUGGED WITH SR1000 OR EQUIVALENT EPOXY.
>
> re,
> ken patel
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|