Hi,
Does anyone have experience from flux free soldering of Sn60/Pb40 on thickfilm. I have tried, but I just can't get the solder to adhere (it peels right off when I'm using a scalpel). I'm using solder preforms and Du Pont's thickfilm paste 4596 (Pt/Pd/Au) in a convection oven with nitrogen atmosphere. I have burnished the thickfilm with an eraser and tried to plasma etch the preforms in argon.
What am I doing wrong? My guess is that there is a thin oxide layer on the preform. Should I use any other method of removing it or should I plasma etch more (I used Ar, 80mTorr, 500W, 13.56 MHz for 5, 10 and 20min).
I'd be very grateful for any tips!
Hakan Tornqvist
Ericsson Microwave Systems
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|