This is a truth that many people overlook. Many WS flux/paste
chemistries use amine- or amino acid-hydrohalide activators and these
have a behaviour like egg white - they dissolve well in cold but set at
higher temps in the presence of water. I recommend a max of 50°C for the
wash cycle with these. Rinse temps can be progressively higher. If a
prewash is possible (or use of a chelating neutraliser, which I
recommend), then this is best at cold.
Brian
Jon Moore wrote:
>
> Janice,
> What temperatures are your wash / rinse cycles? I found white residues
> routinely with water soluble chemistries and OSP panels following wave
> solder, and it turned out that my temperatures were set too high.
>
> Jon Moore
>
> ---------------------------------------------------------------------------------
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF TECHNET
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|