TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Thu, 19 Oct 2000 03:54:14 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (45 lines)
A small clarification:  The most common term used to discuss random vibration environments in the electronic industry is power spectral density [P] [or mean squared acceleration density].  Power spectral density is expressed in squared acceleration units per hertz [G^2/Hz].  Here, "G" is the acceleration expressed in gravity units.  Gravity units are without dimensions [dimensionless???] because, G equals the measured acceleration [a] divided by the acceleration of gravity [g].  In this parlance, an acceleration level of 10g is 10X the acceleration of gravity.  Typically, random
vibration measurements of acceleration, velocity, and displacement are in terms of root mean squared [RMS].

Dave Fish

"Ingemar Hernefjord (EMW)" wrote:

> Of course other gurus are welcome to comment following question, but Werner seems to  be one of those most familiar with life prediction of solder joints and specs.
>
> We have mounted superBGAs, 3 peripherical rows, 600 I/Os, chip down, copper top plate, on SMD multilayer FR-4. We are afraid that somewhere among the produced boards we may have some boards with weak solder joints, probably classical ultrathin weak interface layer between Sn3Ni4 and bulk Ni. PWB is ENIGd. Balls are 95/5, solder is NoClean Sn60. Process is stencil and oven is conveyor N2 heat oven. Cleaning is Citriclean.  In IPC-D-279 app. A you can read about the SMD concerns with starts of cracking, epoxy outbleeding caused by hot solder agains solder mask etc. Now the question.
>
> Q: In A-7.2 Random vibration screening of weak bonds should be done for 10-20 minutes and loaded with 6-10 grams, whole run at -40C. Does not affect good joints, but reveals weak ones. Not easily done, as I can see.
>
> a) what is  6-10 grams loading? Is that momentary top load in grams per BGA solder joint or do you instead mean 6-10 g's?
> b) is this for dummie testing daisy chains, or really meant for produced boards at 10,000 each cost?
> c) general acceleration input on whole board or measured on individual superBGA?
>
> Mebbe a question for Lockheed, Sandia, Rome or like instead, but let's see...
> Thanks in advance
>
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2