IPC-A-610C addresses Press Fit Pins and Connectors in seperate referecnces.
The height spec is 5.2.9. The spec is pretty soft. (Conectors need to meet
form, fit, and fuction requirments. A trial mating of connecor to connector
or to assemlby may be required for final acceptance.)
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David P. Bowers
Sent: Wednesday, October 18, 2000 8:10 AM
To: [log in to unmask]
Subject: [TN] Backplane Press Fit Connector specification
Hi All,
I have ordered copies of the IPC backplane standards but unfortunately they
have not yet arrived.
I need to know what the specification for Press fit connectors are in terms
of how much the connector is allowed to be raised off the PCB.
I have been told the industry standard is 0.25mm but I need conformation of
what IPC states and the IPC number which this is mentioned in.
Any help would be greatly appreciated.
Thanks
David Bowers
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|