In a former life we processed this type of IC in a solder wave without ill
effects. I have not specific data
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bartkowaik Christine
Sent: Wednesday, October 18, 2000 8:25 AM
To: [log in to unmask]
Subject: [TN] waving IC's
I have a double-sided board with 2 SOIC devices on the bottom side along
with a few passive components.
This board has TH components and thus must go through the Solder WAVE
machine. Does anyone have any information on the process of submerging IC's
in the Solder Wave?
Chris
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|