We're in production with a 625 ceramic BGA for a military application. The
BGA was qualified using thermal cycling from -65 C to + 125 C for 1000
cycles. This is a restrained board (7 ppm/C), though.
Thanks,
Jim M.
-----Original Message-----
From: Vincent Bada [SMTP:[log in to unmask]]
Sent: Monday, October 16, 2000 9:24 AM
To: [log in to unmask]
Subject: [TN] BGA for Space Applications
Hi all,
Does anyone as information on the use of a BGA type package
(including CCGA, CSP
...) in a space applications ?
What is the hardest environnement in wich you know a BGA as already
been used ?
Regards,
Vincent Bada
Process Engineer
Alcatel ETCA
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|