Hi,
I'm mounting a 388 package, .050 pith (AMD) BGA onto a .062 board full of
plated vias (.010 dia) throughout the BGA perimeters. Here're my questions:
Should I be concern that solder can flow up during wave solder and cause
shorts on the BGA?
If the BGA locations receives a socket, rather than the BGA, would it make a
difference?
I personally, don't think I have to mask the vias, but QA is concern.
Thank you in advance for any help.