You don't necessarily need to look in the SEM to measure the thickness.
After you've cross-sectioned the joint, etch the surface and then measure
the intermetallic in a metallurgical microscope.
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
2/10/00 18:37
>The only way I know of to determine the IM layer thickness is to
>cross-section the joint, then make an SEM and visually measure the thickness
>on the image.
>
>Timothy Reeves
>QA Manager/Process Engineer
>ECD Circuit Board Division
>
>
>|-----Original Message-----
>|From: Nick.Sanzo [mailto:[log in to unmask]]
>|Sent: Thursday, September 28, 2000 3:06 PM
>|Subject: Solder Joints
>|
>|
>|Hello all
>|I am interested in knowing if anyone is aware of any possible
>|methods or
>|information regarding testing of solder joints. What I am looking for
>|specifically is a way of determining the strength of a joint
>|and a way of
>|determining the properties (ie: thickness) of the
>|intermetallic layer. I am
>|not sure where to find such information. I have attempted
>|internet searches
>|but I have been unsuccessful. Any info would be greatly appreciated.
>|Thanks in advance.
>|
>|Nick Sanzo
>|
>|Operations Engineering-Leitch Technologies
>|416-445-9640 ext. 3852
>[log in to unmask]
>|http://www.leitch.com
>|
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
Best regards,
Martin Christie
Process Engineer
ACW Technology Ltd.,
Hylton Road,
Petersfield,
Hants.
GU32 3XX
Tel: 01730 300000 ext 146
Fax: 01730 266045
e-mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|