> !!!HELP!!!
>
> We are experiencing a strange failure in a circuit board and I hope
> someone can point out the failure mechanism.
> The boards in question fail with trace opens when cold, heat the pin with
> an iron and the open trace reconnects. The boards in question are 0.093"
> thick Getek, 6 layers (4 rout - 2 planes), with 0.015" trace and 0.010"
> spacing (we ain't talkin' high tech here :<) ). We have sectioned the
> holes in question and see really clean plating and pad junctions, no smear
> or nai-heading. Any suggestions as to cause?
>
> Jeffrey A. McGlaughlin, C.I.D.
> Sr. PCB Designer
> Battelle Memorial Institute
> Columbus Ohio
> [log in to unmask]
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|