TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Horaud, Walter" <[log in to unmask]>
Date:
Wed, 6 Sep 2000 14:34:28 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Lee Whiteman <[log in to unmask]>
Subject:
From:
Lee Whiteman <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<EB8B11E11475D411A8F30000EE496589127E34@BDXSRV09>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (84 lines)
Walter Horaud,

For information on BGA's solder masks design rules, I suggest you hit the
following websites:

Amkor:
http://www.amkor.com/customer_center/assembly_and_test/white_papers/index.ht
m

TI: TMS320C6000 BGA Manufacturing Considerations (PDF: 84 KB) (You'll have
to get to TI's website)

Motorola:
http://www.mot-sps.com/cgi-bin/get.pl?/books/apnotes/pdf/an1231*.pdf

In reviewing these documents, they are pretty consistent with Steve
Gregory's reference.

Good Luck

Lee Whiteman
Senior Manufacturing Engineer
ACI / EMPF
Telephone: (610) 362-1200; Ext. 208
FAX: (610) 362-1290
E-Mail: [log in to unmask] <mailto:[log in to unmask]>


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Horaud, Walter
> Sent: Wednesday, September 06, 2000 12:43 PM
> To: [log in to unmask]
> Subject: [TN] Solder mask problems
>
>
> Thechneters,
>
> I'd like to know if there are special design rules for the solder mask on
> PCB.
> Most of PCBs I have seen have pads surrended with a gap and solder mask.
> In our case I have got a PCB with solder mask on the periphery of BGA pads
> (to prevent bridging according to the customer).
> It seems to me that the solder mask on the periphery of pads is not so
> efficient as expected to prevent bridging and it seems to be also
> responsible of the poor mechanical properties of the joint.
> Does anybody have experience with this weird technique (solder mask on the
> periphery of pads)?
>
> Thanks in advance,
>
>
> Walter Horaud
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2