Stephen,
What is the plated material?
Is it Teflon ? We saw such problems on Teflon caused by peeling off the
barrel.
Edward Szpruch
Eltek , Manager of Process Engineering
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
> -----Original Message-----
> From: Stephen R. Gregory [SMTP:[log in to unmask]]
> Sent: ב ספטמבר 11 2000 18:52
> To: [log in to unmask]
> Subject: [TN] Nodules in barrel plating...
>
> Hi ya'll!!
>
> Got another picture for ya to look at for me. We've got some PCB's in
> receiving inspection that has these little nodules in plating inside all
> of
> the barrels. Go to:
>
> http://www.driveway.com/share?sid=e25a88c4.8e904&name=Pictures
>
> and look at Barrelplate.jpg to see what I mean. These are microwave PCB's
> and
> have almost all of the surface area on both sides covered with with solid
> metal planes, and no solder mask.
>
> Is this a normal appearance? The plating inside the barrels look to be a
> much
> lighter color than the plating on the surface planes on the PCB...you can
> see
> that in the picture as well. I don't know what I'm looking at, maybe
> someone
> could help me. I'm being asked if this is okay...I don't know if it is or
> not. I'll try and take a better picture if I can...
>
> Thanks!!
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|