Gentlemen,
What is the current consensus regarding the usable range and minimum
thickness of immersion gold for micro BGA attachment? Is the 2-5 microinch
range usable? Desirable? We have a design and customer requirement that
necessitates the ENIG.
George Carroll
SE&A
Johnson City, TN
##############################################################