A question...you said "...solder mask may be unsuitable...this is quite a common
problem..."
I've not heard of this before, of course I'm a fabricator, not an assembler, but I'm
confident if our customer's were having this problem (i.e. "...this is quite a common
problem") I'm sure they'd be screaming... Would you please expand on those comments,
thanks.
Franklin D Asbell
Brian Ellis wrote:
> OK, Darren. It is not easy to be categorical but I suggest you are
> losing in at least one of two directions, maybe both.
>
> 1) So-called "no-clean" fluxes usually have relatively small amounts of
> activators which tend to sublime/evaporate at temperatures exceeding ca.
> 50°C. It sounds like you may simply not have enough left on the board
> when it hits the wave. Try wicking down the preheat a little at a time
> until the results improve, if this is the case. Perhaps a little more
> flux sprayed on would help, as well.
>
> 2) It may also be that your solder mask is unsuitable or incompatible
> with the flux or has been insufficiently cured. This is quite a common
> problem, especially with some of the glossy masks and dry-film types.
>
> This list is not exhaustive, but you have a 95+++% chance that the
> answer lies above.
>
> Brian
>
> Darren Goh wrote:
>
> >
> >
> > Hi,
> > I would really appreciate some help here..
> > I am running some mixed board (thru holes with SMD) over wave.. after
> > the wave, I discovered almost 80% of the boards are spatter with small
> > lumps of solder dross on the under side... (between three to five
> > counts of them)
> >
> > I am using Tamura no-clean flux and on board preheat temp is peak at
> > 100degree for 10 sec. the whole preheat zone runs at 80 sec..
> >
> > am using Alpha Metal solder bar ..and adopting spray fluxer
> > technology, no clean process..
> >
> > I hope that someone could highlight and share with me the reason (if
> > possible solution) for the formulation of solder dross on the under
> > side of mixed technology boards after wave.
> >
> > thank you very much
> > Darren
> >
> > DID:- (65) 2493448
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|