TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Tracy Black <[log in to unmask]>
Date:
Mon, 18 Sep 2000 14:24:26 -0700
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (73 lines)
The "Dogboneing effect" is caused by excessive plating build up on
generally small parts or on sharp outside corners.  If you look at a part
that has the dogbone on it all or some of the corners will have rounded
corners and they will be beyond the other horizontal or vertical surfaces
that were plated.  You never want to accept any parts that show signs of
this.

That is my two cents on it.

Tracy




                    Richard Gisenia
                    <richardgisenia@        To:     [log in to unmask]
                    YAHOO.COM>              cc:
                    Sent by: TechNet        Subject:     [TN] "Dog Boneing"
                    <[log in to unmask]
                    >


                    09/18/00 02:03
                    PM
                    Please respond
                    to "TechNet
                    E-Mail Forum.";
                    Please respond
                    to Richard
                    Gisenia





I have been informed of a plating issue being called
"dog boneing". What is it, and what is the cause?

__________________________________________________
Do You Yahoo!?
Yahoo! Mail - Free email you can access from anywhere!
http://mail.yahoo.com/

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2