http://www.fciconnect.com , Roger's memoirs are correct .
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, 1 August 2000 23:43
To: [log in to unmask]
Subject: [TN] Connector Pre-tinning (don't have to!)
Hi ya'll!
I just got off the phone with a gentleman from FCI...the plating that is on
the connectors I was talking about yesterday is something they call GXT™,
which is actually palladium nickel alloy with gold flash. I was told by FCI
that it wasn't necessary to pre-tin the connectors, that there wasn't enough
gold on the pins to worry about...
Not that I don't trust them, but do any of you know more about this GXT™
plating? Just trying to learn more...
Thanks!
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|