TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Gary Camac <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 29 Aug 2000 09:45:50 -0500
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (2037 bytes) , gcamac.vcf (315 bytes)
Brian,

I am only seeing this problem on the gold fingers of one assembly.  Haven't had any luck removing it with the solvents I have in house.  You can scratch it off - it seems to be in outer surface of the epoxy.

Gary

Brian Holt wrote:

> Might need to clean the oven.  Could be flux, or some kind of grease or oil dripping off the inside of the oven.  Can it be washed off?  Is it just on the gold fingers?  Is it on just that particular type of board?
>
> -----Original Message-----
> From:   Gary Camac [SMTP:[log in to unmask]]
> Sent:   Monday, August 28, 2000 12:45 PM
> To:     [log in to unmask]
> Subject:        [TN] Staining on edge connector
>
>  << File: gcamac.vcf >> Good morning all,
>
> I have come across something I have never seen before and thought it would be a good idea
> to see what my panel of experts have to say.  I have some assemblies that are showing a
> purple stain in the laminate around the gold contacts of a board edge connector.  Under
> the microscope,  I see no sign of anything on the laminate on the boards from stock.   I
> took a sample of the stock boards and ran them, unpopulated, through the reflow oven and -
> lo and behold - I've got a stain.  The stain seems to be in the epoxy.  A little light
> scratching with a knife blade takes off something purple.
>
> Any ideas as to what I am looking at?
>
> Gary Camac
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################


ATOM RSS1 RSS2