Hi Franklin,
I have question.
Could the bubbles have been caused by volatiles in the flux not being
completely driven off? I remember reading something about this recently
either in Coombs or an old Machine Soldering Workshop.
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials Engineer (Process & Manufacturing)
Warner Robins Air Logistics Center
Avionics Production Division
Precision Attack/Radar/Manufacturing Branch
Engineering Section
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
-----Original Message-----
From: Franklin D Asbell [mailto:[log in to unmask]]
Sent: Monday, August 28, 2000 10:38 AM
To: [log in to unmask]
Subject: [TN] Bubbles in through holes
Help...
A customer has brought a problem to our attention. The yare experiencing
'air bubbles' in through holes after wave soldering.
The copper plating in the hole is averaging 1.25 mils, we have not seen
any compromised hole walls, only bubbles, they even extend up and out of
the hole next to the component leads.
I have uploaded pictures on our website, any assistance would be
appreciated.
These boards were fabricated here in Texas 13 months ago, the customer
did not bake the boards prior to processing. Thanks
You can view these pictures at this link:
http://www.networkcircuits.com/technical.htm
Franklin D Asbell
Network Circuits, Inc.
Irving, Texas 75061
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|