Wed, 23 Aug 2000 07:28:00 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Luis Alcantra <[log in to unmask]>
Subject:
From:
Luis Alcantra <[log in to unmask]>
Content-Transfer-Encoding:
7BIT
Sender:
Parts/Attachments:
text/plain (142 lines)
FORWARDED MESSAGE from fraley , barrie (fraley-b @ SMTP
BF> [log in to unmask]) at 8/23/00 7:21 AM
BF> A good reference
BF> ISBN: 0-471-52277-5
BF> Accelerated testing
BF> By Wayne Nelson
BF> -----Original Message-----
BF> From: David Fish [mailto:[log in to unmask]]
BF> Sent: Tuesday, August 22, 2000 11:29 AM
BF> To: [log in to unmask]
BF> Subject: Re: [TN] Practical Book on ESS (Environmental Stress
BF> Screening).
BF>
BF>
BF> Jean-Paul:  I wouldn't put the Hobbs book on the "practical" shelf ...
BF> the
BF> broad
BF> overview shelf, maybe.  I think Mr. Hobbs is more interested in selling
BF> consulting
BF> services than providing information to practitioners.
BF>
BF> Ken:  It's possible that equipment companies like the following
BF> "shakers"
BF> and "shaker &
BF> bakers" may be able to give you pointers:
BF>
BF> Thermotron 291 Kollen Park Dr Holland, MI 49423 616-393-4580 Fax
BF> 392-5643
BF> www.thermotron.com [log in to unmask]
BF> Protheus Corp 2875 South Tejon St Englewood, CO 80110 800-288-7277 FAX
BF> 303-762-6430
BF> www.proteusdvt.com
BF> QualMark 1329 West 121st Ave Denver, CO 80234 303-254-8800 Fax 4372
BF> www.qualmark.com
BF> Team Corp 11591 Watertank Rd Burlington, WA 98233 360-757-8601 Fax 4401
BF> www.teamcorporation.com
BF> Vibration Test Systems, 10246 Clipper Cove, Aurora, OH 44202
BF> 216.562.5729
BF> fax1186
BF>
BF> If your focus is vibration, "Vibration Analysis For Electronic
BF> Equipment" DS
BF> Steinberg,
BF> J Wiley, which in earlier editions has been an excellent resource, will
BF> be
BF> published in
BF> its 3rd edition this summer.
BF>
BF> Another consultant to consider is: David Hutchins International Limited
BF> Sandhurst House
BF> 297 Yorktown Rd Sandhurst, Camberley, Surrey GU47 0QA UK
BF> www.hutchins.co.uk/
BF>
BF> Dave Fish
BF>
BF> Jean-Paul Clech wrote:
BF>
> Try:
> "Accelerated Reliability Engineering - HALT and HASS" by Gregg K. Hobbs,
> Pub.: Wiley, 2000
> ISBN:0-471-97966-X
> Also, visit: http://www.hobbsengr.com
> JP
> ____________________________________________________
> Jean-Paul Clech
> EPSI Inc., P. O. Box 1522, Montclair, NJ 07042, USA
> SMT / BGA / Flip-Chip / CSP Assembly Reliability Specialists
> tel: +1 (973)746-3796, fax: +1 (973)655-0815
> home page:  <A HREF="http://members.aol.com/Epsiinc1/index.html">epsi</A>
> URL:
> http://members.aol.com/Epsiinc1/index.html
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
BF> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
BF> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
BF>
BF> ##############################################################
BF> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
BF> ##############################################################
BF> To subscribe/unsubscribe, send a message to [log in to unmask] with
BF> following
BF> text in
BF> the body:
BF> To subscribe:   SUBSCRIBE TECHNET <your full name>
BF> To unsubscribe:   SIGNOFF TECHNET
BF> ##############################################################
BF> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
BF> additional
BF> information.
BF> If you need assistance - contact Keach Sasamori at [log in to unmask] or
BF> 847-509-9700 ext.5315
BF> ##############################################################
BF>
BF> ##############################################################
BF> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
BF> ##############################################################
BF> To subscribe/unsubscribe, send a message to [log in to unmask] with
BF> following text in
BF> the body:
BF> To subscribe:   SUBSCRIBE TECHNET <your full name>
BF> To unsubscribe:   SIGNOFF TECHNET
BF> ##############################################################
BF> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
BF> additional
BF> information.
BF> If you need assistance - contact Keach Sasamori at [log in to unmask] or
BF> 847-509-9700 ext.5315
BF> ##############################################################
***** NOTES from Luis Alcantra (LALCANTA @ APSM) at 8/23/00 7:27 AM
 SIGNOFF TECHNET

LUIS ALCANTARA
PROTOTYPE/PROCESS RESEARCH & DEVELOPMENT
[log in to unmask]
(623) 516-3304

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2