TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Brooks Bill <[log in to unmask]>
Date:
Thu, 3 Aug 2000 15:21:41 -0700
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brooks Bill <[log in to unmask]>
Parts/Attachments:
text/plain (117 lines)
Saw the reference to white powder and thought of this article...
http://www.metcal.com/kester/natwtres.html

- Bill Brooks


-----Original Message-----
From: Ryan Grant [mailto:[log in to unmask]]
Sent: Thursday, August 03, 2000 1:31 PM
To: [log in to unmask]
Subject: Re: [TN] Subj: White Tin


flaky white powder....wow!  Sounds like alpha tin, otherwise known as tin
pests.  You better hope not though.  Although, I really can't imagine alpha
tin happening, you better make sure it isn't.

Thanks

Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask]


> -----Original Message-----
> From: Hollandsworth, Ron [SMTP:[log in to unmask]]
> Sent: Monday, July 31, 2000 3:14 PM
> To:   [log in to unmask]
> Subject:      [TN] Subj: White Tin
>
> Hello TechNet:
> We performed some experiments on Immersion White Tin boards and found the
> following . . . .  First, we had no problems with solder paste
> application.
> Second, no problems with vision systems, etc., and part placement.  Third,
> solder joints looked pretty good . . i.e. . no problems.  Here is the
> kicker.  The mounting holes on the top side were white tin.  The mounting
> holes need to be very flat for good contact so we do not apply solder
> paste
> to these holes.  The white tin, after exposure to humidity of the
> environmental chambers looked very oxidized and a flaky white powdery like
> substance was observed.  Also under some RF type connectors, the white
> powdery like substance was observed.  The powdery like flaky substance did
> not show up under any other components only the gold RF connectors.
>
> What experience have any of you had with the immersion white tin process?
> Any ideas, thoughts, etc., on the powdery white substance??? We are going
> to
> have our "product assurance forensic lab" analyze it and see what they
> come
> up with, but we also thought it a good idea to tap the intelligence of the
> TechNet World as well.
>
> Ron Hollandsworth
> ITT
>
>
> ************************************
> If this email is not intended for you, or you are not responsible for the
> delivery of this message to the addressee, please note that this message
> may
> contain ITT Privileged/Proprietary Information.  In such a case, you may
> not
> copy or deliver this message to anyone.  You should destroy this message
> and
> kindly notify the sender by reply email.  Information contained in this
> message that does not relate to the business of ITT is neither endorsed by
> nor attributable to ITT.
> ************************************
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2