TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="ISO-8859-1"
Sender:
Subject:
From:
"Wenger, George M (George)" <[log in to unmask]>
Date:
Thu, 3 Aug 2000 11:03:02 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Wenger, George M (George)" <[log in to unmask]>
Parts/Attachments:
text/plain (84 lines)
Is the copper pad that doesn't coat with solder on the bottom or top of the
board during the HASL operation?  I'm not sure but my guess is that they may
be bottom side features.  If they are bottom side features I might be able
to give you an explanation

Regards,
George
George M. Wenger DMTS
(609)-639-2769 Office (609)-639-3210 Lab
Bell Laboraties Princeton, Engineering Research Center
Supply Network Solutions FMA/AQA/RCA Lab
Po Box 900, Princeton, NJ 085424-0900
Route 569 Carter Rd., Hopewell, NJ 08525



-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, August 03, 2000 7:37 AM
To: [log in to unmask]
Subject: [TN] Copper Pads After HASL


Fellow Technetters,

Occasionally we encounter a phenomenon of copper pads remaining
after HASL.  The copper pad is always a pad that is defined only by
soldermask on a ground plane area. Usually it is square or rectangular and
from
.040" to .080" in dimension. Often small writing in the mask will also
remain
copper.
We've checked:
    developer; strength, temp, spray pressures, rinse pressure, rinse temp
    developed the boards faster, slower, pad side up vs. pad side down

We've checked:
pre clean strength, temp, copper removal, tried faster ,slower , two times
etc.
new flux , old flux, spiked flux(HCL), longer solder dwell

Is it possible that this is caused by the geometry of the pad?  It creates a
sort of inground pool with a mask border. Maybe it doesn't rinse or develop
clean or maybe in the leveler it creates a vapor barrier that doesn't allow
the
solder contact with the copper.
That job at the Ice Cream stand is looking better and better!

Any input appreciated.

Thanks

Brett Austin
Nationwide Circuits Inc.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2