(1) try use most aggressive flux you can find in house
(2) get the profile on the hot side without burning
(3) a little longer pre-heat (slow without damage)
if you still can not solder...it is a hand-solder job...(check the design,
if it is a copy of 1970-early 80s...hand solder the parts!)...my 2
cents...(I am not envy your job..;-)..but been there, done that...It is
mandatory experience for wave solder job......and good luck
jk
At 09:58 PM 8/15/00 EDT, you wrote:
>Hey all...
>
>The last couple of weeks have been interesting to say the least as far as my
>wave soldering goes...(Hey Joyce! Any openings at your new place?...gofer',
>janitor, anything?... ;^)...).
>
>You may have read about my problems with the way pins connect to inner planes
>and all that, but now the last few days I've been trying to wave assemblies
>that have metal heat-sinks bonded to the top of the PCB with the PTH
>components installed on top of the heat-sink and then into the PCB...
>
>Again, I've tried everything that my feeble mind (at this point) can possibly
>do to wave these bloody things...
>
>I'm thinking that designs such as these cannot be wave soldered with any good
>results. Am I wrong in thinking that? Do these designs have to be hand built?
>Am I just spinning my wheels trying to wave solder them?
>
>Gawd, I'm getting beat-up by so many people because I can't figure out how to
>wave these pieces of...of...of..."work"...
>
>-Steve Gregory-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|