Scott,
Why would solder be trapped in the vias? If the board is SMOBC, with the
vias tented, there should be no problem. But since there is, could you
provide more data on how the board is constructed? Is it SMOBC, or is mask
applied after HASL? What kind of solder mask is being used? What diameter
(finished) are the vias? Is the print specifying the board specific enough
for the finished bare board, or is it nebulous? (How many fabricators out
there get nebulous prints? Nobody? ;-)
One solution may be opening (un-tenting) the vias. This may pose a problem
though with ICT.
Roger M. Stoops, C.I.D., PCB Designer
Spectra Precision Inc./Trimble Navigation Ltd.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511
"Lefebvre,
Scott" To: [log in to unmask]
<Scott_Lefebvr cc:
[log in to unmask]> Subject: [TN] Solder masked Via problems
Sent by:
TechNet
<[log in to unmask]
RG>
08/10/00 03:18
PM
Please respond
to "TechNet
E-Mail
Forum.";
Please respond
to "Lefebvre,
Scott"
I have a problem with via's that have been masked over having trapped
solder in the via's after HASL. The solder that is in the via's is
surfacing after we reflow the bottom side of the board. I have not had
this problem before and wanted some advice from all of you. I am sending
this message again due to the lack of response I got. Any help or advice
would be greatly appreciated!
Thank you,
Scott Lefebvre
[log in to unmask] <mailto:[log in to unmask]>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|