What are the causes of the internal crack on only on layer 5? Most of the
cracks found were on via holes extending into the laminate (no
delamination!). Prepreg used at layer 5 is 3 sheets of 1080 of FR406 (these
3 will give a total of .008" thickness to overall thickness of .093").
Loaded boards failed at ICT that prompted us to do some investigation. What
should I do as an OEM customer on my own as my fab house and assembly house
won't take responsibility easily. Following information may help you
understand my board structure.
# of layers: 12
SIG/GND/SIG/GND/SIG/3.3V/VCC/SIG/GND/SIG/GND/SIG
1oz copper used on all layers except first and last which plated to 1oz final.
re,
ken patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################