Hi Justin,
It seems you're used to weighing the parts before deciding about double reflow. Than you have probably noticed that there exist large weight-variations between different components with similar body-types. Your TSOP 28T could be easily be twice as heavy as Ryan's or Steve's !!
Still, for TSOP's, personally I wouldn't worry. But for QFP's or PLCC's it can be a dangereous thing to trust on somebody else's experiences.
Kind Regards,
Daan Terstegge
SMT Centre
Signaal Communications
Unclassified mail
Personal Website: http://surf.to/smtinfo
>>> Ryan Grant <[log in to unmask]> 07/07 12:30 am >>>
no sweat.
Unless the component is made out of alumina or has a heatsink slug, it will
easily stay on the board by surface tension alone. (I have never seen a
TSOP made out of alumina or with a heat sink. But never say never!)
Thanks
Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask]
> -----Original Message-----
> From: Justin Braime [SMTP:[log in to unmask]]
> Sent: Thursday, July 06, 2000 4:03 PM
> To: [log in to unmask]
> Subject: [TN] Component weights for double-sided reflow
>
> Hi All,
> Can anybody tell me if it is possible to perform double-sided reflow with
> TSOP 28T or 32T components on the bottom-side?
> I could work it out myself if I could only find the component weights!
> The prouct is at the design stage, so I don't have any components I can
> weigh :-(
>
> Thanks in advance!
>
> Justin Braime
> Compuspec Industries Ltd
> Auckland, New Zealand
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|