Hi Tom,
I would look at two item to start.
First verify that your parts are not bottoming out on vias underneath the
part. Second is to see if the leads are made of alloy 42.
Best of luck
Hector Valladares
Honeywell -SASSO
Production Staff Engineer
727.539.3683 voice
[log in to unmask]
-----Original Message-----
From: Thomas Han [mailto:[log in to unmask]]
Sent: Tuesday, July 18, 2000 12:17 PM
To: [log in to unmask]
Subject: [TN] Reflow Issue
Hi all,
I have been noticing on our last batch of boards that we ran, some of the
tsop flash chips were not reflowing properly. I am not getting very good
toe fillets on the chips and some appear as though they are just sitting on
top of the reflowed solder. This board has a good component mix(i.e. BGA,
QFPs, PLCCsocket, SOICs, total(325-350)). Other components reflow fine,
but for some reason these TSOPS are not. Is there something that we are
overlooking?
Your input would be greatly appreciated. Thanks in advance
Tom
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|