Evidently my posting fell through the cracks somewhere along the line
because I received a message stating that it was being returned for reasons
I don't understand. Whatever!
The ideal material to remove tape residue is called "Goo Gone". I use it at
home and I have seen librarians use it to remove residue from labels put on
library books. It does the job and is available at local stationary outlets.
Ron Dieselberg
BAE SYSTEMS
Cincinnati Electronics Corp.
##############################################################