Do you have any information as to whether this is Omikron?
:-) -----Original Message-----
:-) From: TechNet [mailto:[log in to unmask]]On Behalf Of
:-) Hollandsworth, Ron
:-) Sent: Monday, July 31, 2000 5:14 PM
:-) To: [log in to unmask]
:-) Subject: [TN] Subj: White Tin
:-)
:-)
:-) Hello TechNet:
:-) We performed some experiments on Immersion White Tin boards
:-) and found the
:-) following . . . . First, we had no problems with solder
:-) paste application.
:-) Second, no problems with vision systems, etc., and part
:-) placement. Third,
:-) solder joints looked pretty good . . i.e. . no problems.
:-) Here is the
:-) kicker. The mounting holes on the top side were white tin.
:-) The mounting
:-) holes need to be very flat for good contact so we do not
:-) apply solder paste
:-) to these holes. The white tin, after exposure to humidity of the
:-) environmental chambers looked very oxidized and a flaky
:-) white powdery like
:-) substance was observed. Also under some RF type
:-) connectors, the white
:-) powdery like substance was observed. The powdery like
:-) flaky substance did
:-) not show up under any other components only the gold RF connectors.
:-)
:-) What experience have any of you had with the immersion
:-) white tin process?
:-) Any ideas, thoughts, etc., on the powdery white
:-) substance??? We are going to
:-) have our "product assurance forensic lab" analyze it and
:-) see what they come
:-) up with, but we also thought it a good idea to tap the
:-) intelligence of the
:-) TechNet World as well.
:-)
:-) Ron Hollandsworth
:-) ITT
:-)
:-)
:-) ************************************
:-) If this email is not intended for you, or you are not
:-) responsible for the
:-) delivery of this message to the addressee, please note that
:-) this message may
:-) contain ITT Privileged/Proprietary Information. In such a
:-) case, you may not
:-) copy or deliver this message to anyone. You should destroy
:-) this message and
:-) kindly notify the sender by reply email. Information
:-) contained in this
:-) message that does not relate to the business of ITT is
:-) neither endorsed by
:-) nor attributable to ITT.
:-) ************************************
:-)
:-) ##############################################################
:-) TechNet Mail List provided as a free service by IPC using
:-) LISTSERV 1.8c
:-) ##############################################################
:-) To subscribe/unsubscribe, send a message to
:-) [log in to unmask] with following text in
:-) the body:
:-) To subscribe: SUBSCRIBE TECHNET <your full name>
:-) To unsubscribe: SIGNOFF TECHNET
:-) ##############################################################
:-) Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|