TECHNET Archives

July 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Hans Rohr <[log in to unmask]>
Date:
Sat, 29 Jul 2000 11:04:05 +0100
Reply-To:
Mike Fenner <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="Windows-1252"
From:
Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
All the major electronic/microelectronic adhesive suppliers have
screenable Ag epoxies you could sort of use for this, but I would be a
bit sniffy about it.
Its been done before, but personally I would not recommend it except
as a short term/prototyping type fix. Not really good for a long term
high reliability assembly, probing on to Ag epoxy is not necessarily
going to produce a consistent result either. Does your customer have
prior experience on this assembly showing results are good enough for
the intended application?

Mike

----- Original Message -----
From: "Hans Rohr" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 26, 2000 2:10 AM
Subject: [TN] Plugging Vias With Conductive Epoxy


> One of our customers wants us to plug vias (.016-.020") with a
> conductive epoxy material.  The board is finished with white tin so
> plugging with solder is out. The vias do not have to be completely
> filled but the plugs must be strong enough to withstand test probe
> pressure.  The epoxy filled vias will be used as test points.  We
have
> used carbon and silver epoxy on conductive surfaces but never to
plug
> holes.  Has anyone ever done this and can you suggest a conductive
epoxy
> that can be screened on?
>
> Hans Rohr
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2