John,
We have seen the PTH via crack (circumferential) which results into open
during ICT. At that moment our boards are gone thr' two reflow cycle (225c
max) and one wave cycle.
How can I select chamber profile so that it will weed out bad one? Is there
any guide lines? My boards are loaded with components and need resolution ASAP.
re,
ken patel
At 12:03 PM 7/20/2000 -0400, you wrote:
>Ken mentions:
>
>> Reliability/Quality Expert,
>> How can I select the thermal stress/shock profile for loaded board if I
>want
>> to precipitate the fab problem. Boards are functionally passed but belongs
>> to suspect date code.
>>
>> I am looking for a profile in the following format.
>
>Hi Ken,
>
>Before you do any testing, a good, root cause failure analysis is
>required before specifying a failure acceleration method.
>
>Once you've conclusively identified the specifc cause of your
>module failure, you can tailor a stress test to weed out that
>specific problem (or fix the root cause failure reason, better yet!)
>
>Without the root cause failure identified, you may end
>up spending a lot of money, and potentially ruining a lot
>of good modules doing accelerated life/reliability testing,
>with minimal return.
>
>Rgds
>John
>
>
>-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
>John Brewer
>Supervisor, Component Engineering
>Raleigh, NC
>(919)-266-8870
>[log in to unmask]
>-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
>
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|