Hans,
I believe that Mike is referring to EC-7M by Petroferm. Not only is it s
good board cleaner, but it will remove adhesive residue. You get it packaged
in the MicroCare, which would be the best application. MicroCare's website
is: http://www.microcare.com/. Some of their other cleaning solvents may
work as well, but from personal experience, EC-7M will remove adhesives.
A word of caution. It does have a heavy smell (it's made from orange peels
and is concentrated) and some operators will be sensitive to it.
Lee Whiteman
Senior Manufacturing Engineer
ACI / EMPF
Telephone: (610) 362-1200; Ext. 208
FAX: (610) 362-1290
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Hans, you should find that a terpineol based flux remover (the ones
that smell
of oranges or pine) will work excellently on sticky labels. White
spirit (paint thinner) should also be OK but at a reduced rate.
Mike
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Hinners Hans Civ
> WRALC/LYPME
> Sent: Thursday, July 13, 2000 4:41 PM
> To: [log in to unmask]
> Subject: [TN] Adhesive Remover for artwork
>
>
> Hey Gang,
>
> I'm looking for an adhesive remover.
>
> We're using a new label printer to image the batch numbers on the panels.
> Only problem, the labels are leaving adhesive on the artwork when we pull
> them off. I already tried Chemtronics adhesive remover and it
> just smeared
> the glue around. So, before I start making a bunch of calls or trying
> household cleaners I thought I'd ask this illustrious body.
>
> Thanks,
>
> Hans
>
> ~~~~~~~~~~~~~~~~~~~
> Hans M. Hinners
> Materials (Process & Manufacturing) Engineer
> Warner Robins Air Logistics Center
> Avionics Production Division
> Manufacturing Branch
> 380 Second Street, Suite 104
> Building: 640, Mail Stop: LYPME
> Robins AFB, GA 31098-1638
> Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
> mailto:[log in to unmask]
> http://www.robins.af.mil
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|