Hans,
Did you check the test method? Could there be 11 plies instead of 10,
or was the prepreg style 2116 instead of 2113?
Glenn
Hinners Hans Civ WRALC/LYPME <[log in to unmask]> Wrote:
|
| Hello Cyber junkies!
|
| They just put me in charge of our Drill operation and I have my first
| question.
|
| Our Scale Flow Test for a lot of PGFK 2113 gave us an average thickness of
| 3.9 mils instead of the expected 3.5 mils.
|
| What does this mean?
|
| I'm guessing the prepreg either didn't flow enough or gelled to quickly.
|
| I need to figure out if the material is still good or if we just need to
| tweak the board stackup so we don't exceed max tolerance.
|
| Thanks!
|
| Hansie
|
| ~~~~~~~~~~~~~~~~~~~
| Hans M. Hinners
| Materials (Process & Manufacturing) Engineer
| Warner Robins Air Logistics Center
| Avionics Production Division
| Manufacturing Branch
| 380 Second Street, Suite 104
| Building: 640, Mail Stop: LYPME
| Robins AFB, GA 31098-1638
| Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
| mailto:[log in to unmask]
| http://www.robins.af.mil
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|