> I'd like to hear from anyone who has evaluated or is using Zestron Vigon
> A-200. We are evaluating it as a semi-aqueous defluxing agent for RMA. In
> some very preliminary cleaning trials, it looks interesting. I was just
> wondering who else is using it and how things were going.
Mary,
If I recall correctly, Zestron was one of the cleaning agents examined in the
IPC Cleaning and Cleanliness Test Program, Phase 2. The testing was done by
EMPF and you may be able to get a copy of the report from their librarian.
Check www.aci-empf.org (I think). Check and make sure that formulation is
the same.
Doug Pauls
CSL
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|