We have used Siemens SN29500 Norm. The results meets quite well the actual
field failure rate.

B.R.
Jarmo Kiiski

> -----Original Message-----
> From: Kang Zhang [SMTP:[log in to unmask]]
> Sent: 13. kesäkuuta 2000 08:41
> To:   [log in to unmask]
> Subject:      [TN] Reliability Prediction Methods
>
> Hello all
>
> Two questions:
>
> 1. Is there any big difference in reliability prediction results between
> using MIL-HDBK-217F notice2 and using Bellcore? I just try MIL. Using
> Bellcore can get "better" MTBF or "worse"?
>
> 2. Except the above two, are there any other methods to predict the
> reliability of electronic components, such as FET, Bipolar?
>
> Any inputs are very welcome. Thanks in advance!
>
> Kang
>
>
> ________________________________________________________________________
> Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2