That sounds like it would work... A lot cleaner than introducing the
chemicals to an assembled board. Might want to apply a low tack adhesive
backing after Ni/Ag plate to retain the die cut disks after punching...
Punch could be a steel rule die which is cheap to make and lasts a long
time... How many boards will need to be reworked?
It might justify the cost of the die, (about 250 bucks)... I think.
- Bill Brooks
-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Friday, June 09, 2000 1:07 AM
To: [log in to unmask]
Subject: Re: [TN] still confused
OK, Ralph, I may have an answer which will satisfy everybody and provide a
reliable
solution. Buy some 50 micrometre rolled copper foil and have it
electroplated on one
side with, say 5 um Ni and 1 um Au. This would not be expensive. Stamp out
contact-size
disks. Put a drop of RMA or "no-clean" flux on the HASL contacts, place a
disk onto it,
gold side out, and heat until the HASL solder melts and the disk becomes +/-
integral
with the assembly. Et voila!
Heating can be via focussed IR, thermode, hot gas or even, with care, a
soldering iron.
Brian
Ralph Richart wrote:
> We have answers....
>
> So I had a long talk with my customer this morning to provide input
> based on the invaluable advice from you all.
>
> I said - "is there a specific reason for choosing 3-8u" of immersion
> gold over tin/lead solder?"
> He said - "absolutely, the gold provides corrosion resistance, the gold
> does not"
> I said - "even such a thin amount - only 3-8u"?"
> He said - "definitely, all we need is the coverage, the thickness is
> irrelevant"
>
> Is this true?
>
> Needless to say, we are rebuilding the parts as we speak. Rework sounds
> difficult to say the least, although I may try to come up with some
> scheme for fun as they have a bunch of boards that are no good right
> now.
>
> thanks for all the help.....
>
> ralph
>
> PS - more on the larrylobster story later; it's more silly than anything
> else. Paul's poem may soon become our own, however. Very funny!
>
> Off to build some boards....
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|