Yes we have without any problem.
We used a Soltec prismawave Soldering Machine with smartwave (main wave
ondulation) and chip wave on. We also use Alpha Metals "Wave survivor"
no-clean flux SLS65 and forced convection heating with great succes.
Alain Mathieu
Electroline Equipment Inc
[log in to unmask]
-----Original Message-----
From: Ross, Mark [mailto:[log in to unmask]]
Sent: Thursday, June 29, 2000 9:37 AM
To: [log in to unmask]
Subject: [TN] Anyone wave soldering SMA (DO-214AC) diodes?
Anyone out there wave solder SMA style diodes? These for example are the
electrical equivalent of the 1N4004 diode but not in a glass MELF packages,
the package is flat so it does not roll around. Any comments would be
appreciated. Thanks.
Mark Ross
Electronic Design Engineer
Innovative Home Products Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|