Hi Bill - take a look at the May 2000 issue of SMT magazine, "Designing
with CBGAs: An Experimental Approach" authored by Richard Morgen. The
article may be helpful for your application. Can you use a plastic BGA
instead of a ceramic BGA? The PBGAs have an overall longer thermal cycle
life than the CBGAs in most applications. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bill Robinson <[log in to unmask]>@IPC.ORG> on 06/01/2000 08:18:27 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Bill Robinson <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] BGA application
Good Morning,
I have an application that requires using a 474 ball and a 250 ball
CBGA in a military environment. These will be mounted on a random
kevlar Polyimide board, soft bonded to an aluminum thermal core. Has
anyone had similar experience, and what have you learned? Also will I
need to underfill the parts? If so, what would you recommend for an
underfill material? Thanks in advance for any help.
Bill
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|