TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brunker Ed <[log in to unmask]>
Date:
Tue, 27 Jun 2000 14:00:01 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (49 lines)
Ed:  Try

"Vibration Analysis For Electronic Equipment" DS Steinberg, J Wiley
*  3e (047137685X) will be published this summer
*  2e 1988  (0471633011) at SMTA Book Store
*  1e  (0471821004) at your favorite used book store about $45

Dave Fish


Brunker Ed wrote:

> There have been millions of hours testing the reliability of electronic
> assemblies through thermal cycling. There are countless authorities on this
> subject. The reliability of assemblies with regard to mechical shock and
> vibration present a different scenario. Are there any references for
> information regarding work done in this field?
> Regards
> Edward Brunker
> Principal Process Engineer
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2