TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Mon, 26 Jun 2000 10:40:04 +1000
MIME-Version:
1.0
X-To:
Richard Tilbrook <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (94 lines)
I knew i could not be that blind (no pumpkin home brews here);
Richard , as Eric astutely pointed out your title is Ag,
but in text you talk about gold .

The baking of silver with organic coat obviously very much differs from
gold's;
was it a typo or did you asked for silver ,
(in that case i'd understand your apprehension easier, hangovers too)



thanks           paul



-----Original Message-----
From: Richard Tilbrook [mailto:[log in to unmask]]
Sent: Wednesday, 21 June 2000 17:30
To: [log in to unmask]
Subject: Re: [TN] Ag on Ni - effect of baking


NEW MESSAGE:

Hi folks,
Sorry, I wasn't feeling well yesterday and did not explan myself at all -
the
reason I asked about baking is that we reflowed one side of a surface mount
board
(gold on nickel); we then stored it in a 45'C oven as we were expecting the
remaining parts to arrive for this very urgent job. They unexpectedly took a
week.
They even more unexpectedly didn't want to reflow properly when we tried
reflowing.
I suggested "passivation" as something for the person who brought me the
problem to
think about, though I must confess that being an industrial placement
student, I am
not best equiped to make that kind of judgement. As I try to follow many of
your TN
discussions, and occasionally add when I feel able, I was sure you'd be able
to
give better reasons as to the cause and suggestions for either prevention or
cure.

Thanks and Regards,

Richard Tilbrook



PREVIOUS MESSAGE:

Hi technetters,
I'm hoping to find out a bit more about the effect of baking (at 45 deg. C)
on
boards with gold on nickel.
I would be grateful for any info on the sibject, including times,
temperatures and
effects, such as passivation.

Thanks,

Richard TIlbrook

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2