TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Le Dai Tri <[log in to unmask]>
Date:
Fri, 23 Jun 2000 12:17:38 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (122 lines)
Tri

Very little scientific work has been done on this. The original doc taking figures out
of a hat for G-10 laminate was MIL-P-275x, now, I think, partially incorporated into
IPC-P-275x but, to the best of my knowledge, there has been little more recent done
than this 30+ year-old data, which applies to all applications.

In 1988, I published a paper giving evidence of reversible ion migration within FR-4
laminates at voltage gradients as low as 10 V/mm with recovery times of several hours.
This does not mean that they should not be used at such gradients for most
applications, but at 100 V/mm there was some small evidence of permanent changes. My
feeling is that, above this, there could be a risk.

Brian

Le Dai Tri wrote:

> Dear Brian,
>
> Could you tell me specific voltage gradient spec. for each kinds of PWB:
> handheld, consumer, mother board ...?
> Which document may I refer ? (IPC, MIL ...)
>
> Best regards,
> Tri'.
>
> ----- Original Message -----
> From: Brian Ellis <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, June 22, 2000 6:08 PM
> Subject: Re: [TN] Electrical testing of bare board
>
> > Howard
> >
> > I presume by 3,5 mil, you mean 0,0035", equivalent to about 80
> micrometres. Putting 250
> > V across this, with or without mask, gives a voltage gradient of about
> 3000 V/mm which
> > is HORRENDOUS. A typical acceptable voltage gradient without mask is about
> 100-150
> > V/mm, maybe double that with mask, if all the best conditions are united.
> If your
> > substrate has absorbed any humidity (and it is likely that it will have
> done), you will
> > be pulling apart any ionics in the material. At the best, you will damage
> it. At the
> > worst, it will simulate an arc welder. Please don't do it.
> >
> > Brian
> >
> > Howard Lin wrote:
> >
> > > Hi TechNetters,
> > >
> > > We do some testing  of  bare board right now.  Can anyone point out what
> > > different between board with solder mask and without solder mask  on
> > > electrical testing process? If we apply 250 voltage on 3.5 mil spacing
> > > pattern , will it damage electrical character? Is there copper migration
> > > occuring during 250 voltage testing?
> > >
> > > Howard Lin
> > >
> > > ##############################################################
> > > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > > ##############################################################
> > > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> > > the body:
> > > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > > To unsubscribe:   SIGNOFF TECHNET
> > > ##############################################################
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > > information.
> > > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > > 847-509-9700 ext.5315
> > > ##############################################################
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> > the body:
> > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > To unsubscribe:   SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > information.
> > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2