Ken - I suggest you consider using Sn62 solder to slow down the leaching of
the Palladium-Silver termination. Do you have a barrier layer or is this
just a single layer termination? If a single layer, you may only get one
reflow cycle out of the termination before it dissolves into
non-wettablility. Why don't you use a standard 3-layer termination?
Ed Valentine
Electronics Manufacturing Solutions
8612 Mourning Dove Road, Raleigh, NC 27615
Phone: (919) 270-5145, Fax: (919) 847-9971
Email: [log in to unmask]
Website: http://www.ems-consulting.com
----- Original Message -----
From: Chafin, Ken G. <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, June 22, 2000 5:45 PM
Subject: [TN] Termination/Soldering Combination
> We are planning to solder some surface mount capacitors with
> palladium-silver terminations on our printed circuit assemblies using
> tin-lead (SN63/37) solder.
>
> Does anyone know of any long term reliability problems with this
termination
> alloy/soldering combination?
>
> We can get these capacitors with nickel-tin terminations.
>
> Given that our solder is tin-lead, does anyone know whether one of these
> termination alloys would be preferable to the other?
>
> Thanks for any insight you may be able to provide.
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|