Ruby,
You'll be looking at ceramic. Possibly LTCC, probably 96% Alumina with AuSn
(80\20 - 283C)
solder in inert atmosphere. Contact me off line if you'd like but I will be
away through June 21.
Regards, Bruce Misner
> ----------
> From: Ruby Hazen[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Ruby Hazen
> Sent: Friday, June 16, 2000 6:52 PM
> To: [log in to unmask]
> Subject: [TN] High Temperature PWB
>
> Hello all
>
> We are looking for a printed wiring board system which can operate at
> +260C.
> Any recommendations and inforamtion are very welcome.
>
> Thanks a lot!
>
> R.H.
> ________________________________________________________________________
> Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|